Particle size of silicon carbide | GC1200 and GC1500, can be customized | |||
|
||||
Density (kg/l) | 1.62-1.64, can be customized | |||
|
||||
Viscosity (mPa.s) | 180-350, can be customized | |||
|
||||
Standard package | Barrelled package is used in trial period with 1 ton per barrel, and two barrels can be stacked up during transportation | |||
|
||||
Storage | After delivery, the slurry is stored in client’s stirring vat, and should be stirred for 30 minutes every three hours for maintenance. Continuous stirring for 90 minutes is required before being used in the machine | |||
|
||||
Disposal of waste slurry | Waste slurry is independently stored in the specific Fundant barrel (mixing with other slurry is prohibited!) | |||
|